Westmag Technology Corporation Limited
Westmag Technology Corporation Limited
SmCo Magnets with High Working Temperature
  • SmCo Magnets with High Working Temperature
  • SmCo Magnets with High Working Temperature
  • SmCo Magnets with High Working Temperature
  • SmCo Magnets with High Working Temperature
  • SmCo Magnets with High Working Temperature
  • SmCo Magnets with High Working Temperature
  • SmCo Magnets with High Working Temperature
  • SmCo Magnets with High Working Temperature
SmCo Magnets with High Working Temperature
SmCo Magnets with High Working Temperature
SmCo Magnets with High Working Temperature
SmCo Magnets with High Working Temperature
SmCo Magnets with High Working Temperature
SmCo Magnets with High Working Temperature
SmCo Magnets with High Working Temperature
SmCo Magnets with High Working Temperature

SmCo Magnets with High Working Temperature

Payment Type:
Telegraphic Transfer (TT, T/T)
Quantity:

Your message must be between 20 to 2000 characters

Contact Now
Basic Info
Basic Info
Payment Type: Telegraphic Transfer (TT,T/T)
Product Description
Product Description
  • Characteristics:
    • SmCo magnet is a high performance low temperature coefficient permanent magnet, made of samarium and cobalt and other rare-earth elements
    • Its biggest advantage is its high working temperature (500°)
    • It need not to be coated because it is difficult to be eroded and oxidized
  • Applications: widely used in motors, watch, transducers, instruments, positional detector, generators, radar and more
  • SmCo5:
    • Temperature coefficient of Br: -0.05%/°C
    • Temperature coefficient of iHc: -0.3%/°C
    • Curie temperature: 700-750°C
    • Density: 8.2-8.4g/cm³
    • Vickers hardness: 450-500 HV
    • Working temperature: 250°C
  • Sm2Co17:
    • Temperature coefficient of Br: -0.03%/°C
    • Temperature coefficient of iHc: -0.2%/°C
    • Curie temperature: 800-850°C
    • Density: 8.3-8.5g/cm³
    • Vickers hardness: 500-600 HV
    • Working temperature: 350°C
  • SmCo magnet is a high performance low temperature coefficient permanent magnet, made of samarium and cobalt and other rare-earth elements
  • Its biggest advantage is its high working temperature (500°)
  • It need not to be coated because it is difficult to be eroded and oxidized
  • Temperature coefficient of Br: -0.05%/°C
  • Temperature coefficient of iHc: -0.3%/°C
  • Curie temperature: 700-750°C
  • Density: 8.2-8.4g/cm³
  • Vickers hardness: 450-500 HV
  • Working temperature: 250°C
  • Temperature coefficient of Br: -0.03%/°C
  • Temperature coefficient of iHc: -0.2%/°C
  • Curie temperature: 800-850°C
  • Density: 8.3-8.5g/cm³
  • Vickers hardness: 500-600 HV
  • Working temperature: 350°C